Polymer Property : Melt Flow = 26.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 26.3 g/10 min

@Load 5.00 kg,
Temperature 280 °C
26.3 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..
Melt Flow 26.3 g/10 min

@Temperature 190 °C
26.3 g/10 min

@Temperature 374 °F
Cyclewood Solutions Xylomer™ XM1-LA Injection Molding Compostable Resin
100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an ab..