Material Notes:
100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an abundant, natural byproduct of the paper manufacturing process, blended with other compostable polymers. Xylomer™ pellets have been demonstrated in injection molding and vacuum forming processes to create samples of cups and bowls.Information provided by Cyclewood Solutions.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Melt Flow 26.3 g/10 min

@Temperature 190 °C
26.3 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength 11.64 MPa
1688 psi
Elongation at Break 3.7 %
3.7 %
Flexural Modulus 0.848 GPa
123 ksi
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in