Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 21.92 g/10 min @Load 2.16 kg, Temperature 250 °C |
21.92 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |