Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.96 g/10 min | 2.96 g/10 min | ASTM D1238 |
Multibase Multi-Flam™ 0102 Natural PP Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |