Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.500 - 2.30 g/10 min | 0.500 - 2.30 g/10 min | Average value: 0.865 g/10 min Grade Count:10 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |