Physical Properties Metric English Comments
Melt Flow 0.500 - 190 g/10 min
0.500 - 190 g/10 min
Average value: 26.5 g/10 min Grade Count:126
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..