Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.1 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.1 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Melt Flow | 17.1 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.1 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |