Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.200 - 155 g/10 min | 0.200 - 155 g/10 min | Average value: 48.3 g/10 min Grade Count:27 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |