Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15.51 g/10 min | 15.51 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 9502 BLK , 7% Filler Content The moisture content is 0.02%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |