Physical Properties Metric English Comments
Melt Flow 15.2 g/10 min
15.2 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Pro® 4810 C White 47.7% Filler Content Polypropylene
Moisture content is 0.04%. Data provided by Multibase.
Melt Flow <= 15.2 g/10 min

@Load 10.0 kg,
Temperature 380 °C
<= 15.2 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..