Physical Properties Metric English Comments
Melt Flow 130 g/10 min

@Load 5.00 kg,
Temperature 316 °C
130 g/10 min

@Load 11.0 lb,
Temperature 600 °F
ASTM D1283
Chevron Phillips Ryton® PR06 Polyphenylene Sulfide Resin  (discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
Melt Flow 130 g/10 min

@Load 2.16 kg,
Temperature 190 °C
130 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2328 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 130 g/10 min

@Load 2.16 kg,
Temperature 160 °C
130 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melt Flow 130 g/10 min
130 g/10 min
ASTM D1238
ExxonMobil Escorene™ UL 12530CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 12530CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot..
Melt Flow 130 g/10 min

@Load 2.16 kg,
Temperature 275 °C
130 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Melt Flow 130 g/10 min

@Load 5.00 kg,
Temperature 275 °C
130 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B27 E 01 PA6 (Dry)
Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German..