Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 116 g/10 min | 3.00 - 116 g/10 min | Average value: 35.7 g/10 min Grade Count:24 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |