Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.73 g/10 min @Load 2.16 kg, Temperature 190 °C |
11.73 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1183 |
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f.. |