Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.6 g/10 min @Temperature 230 °C |
11.6 g/10 min @Temperature 446 °F |
ASTM D1238 |
Asia Technology Pioneers CAP 101 PP Nanocomposite Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Melt Flow | 11.6 g/10 min @Temperature 230 °C |
11.6 g/10 min @Temperature 446 °F |
ASTM D1238 |
Asia Technology Pioneers CAP 102 PP Nanocomposite Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |