Polymer Property : Melt Flow = 11.6 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 11.6 g/10 min

@Temperature 230 °C
11.6 g/10 min

@Temperature 446 °F
ASTM D1238
Asia Technology Pioneers CAP 101 PP Nanocomposite
Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..
Melt Flow 11.6 g/10 min

@Temperature 230 °C
11.6 g/10 min

@Temperature 446 °F
ASTM D1238
Asia Technology Pioneers CAP 102 PP Nanocomposite
Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di..