Polymer Property : Melt Flow = 108 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 108 g/10 min

@Pressure 0.655 MPa
108 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
PolyOne Geon™ 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® 136 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy saving and the ability to work with heat sensitive substrates. The ..