Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Noble Polymers Forte™ 12HPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Melt Flow | 10.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Data |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Melt Flow | 10.4 g/10 min @Load 6.60 kg, Temperature 337 °C |
10.4 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 10.4 g/10 min @Load 2.16 kg, Temperature 275 °C |
10.4 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Melt Flow | 10.4 g/10 min @Load 6.60 kg, Temperature 337 °C |
10.4 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 2110N PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |