Physical Properties Metric English Comments
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex APEX® 130 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Appliance Wire Jacketing; Building Wire Jacketing; Flexible Cord Jacketing; Wire and Cable App..
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer
Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:..
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Melt Flow 1.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
ExxonMobil Escorene® LD 720.62 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Melt Flow 1.60 - 23.0 g/10 min
1.60 - 23.0 g/10 min
Average value: 5.26 g/10 min Grade Count:27
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Melt Flow 1.60 - 12.0 g/10 min
1.60 - 12.0 g/10 min
Average value: 5.35 g/10 min Grade Count:13
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded