Physical Properties Metric English Comments
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC BF315 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesApplications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC ST318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica..
Melt Flow 0.40 - 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 - 1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers ABS 9401 Injection Molding Grade, Ultra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 0.40 - 1.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.40 - 1.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 9501
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati..