Physical Properties Metric English Comments
Melt Flow 0.67 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.67 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 97B HDPE Extrusion Resin  (discontinued **)
Features: Excellent stretchability, high strength and gloss, excellent processability, high stiffness, gel free.Applications: Industrial woven bags, tarpaulins.Data provided by the manufacturer.
Melt Flow 0.67 - 0.99 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.67 - 0.99 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GD 5150 K HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 0.67 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.67 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin  (discontinued **)
Features: Good impact strength, easy processability, high ESCR.Applications: Small part blow molding, high ESCR HIC applications.Data provided by the manufacturer.