Polymer Property : Melt Flow = 0.50 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 102-15 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 102-16 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 102-17 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 102-21 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 102-23 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 153-15 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 153-21 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 153-23 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 153-17 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Melt Flow 0.20 - 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Breplast Bretene HD Bottles Flakes High Density Polyethylene
Recovered polyethylene compositeInformation provided by Breplast S.p.A.
Melt Flow 0.20 - 0.50 g/10 min
0.20 - 0.50 g/10 min
Kazanorgsintez 153-16 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..