Physical Properties Metric English Comments
Melt Flow 0.15 - 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC PF150 HDPE
Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall..