Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.15 g/10 min | 0.15 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 4102 High Density Polyethylene Resin Petromont HDPE 4102 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for general use in large diameter light weight drainage tubing applicat.. |
|||
Melt Flow | 0.15 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9642 HDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Melt Flow | 0.15 g/10 min @Load 2.16 kg |
0.15 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Melt Flow | 0.15 g/10 min | 0.15 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Melt Flow | 0.15 - 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 - 0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC PF150 HDPE Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall.. |
|||
Melt Flow | 0.15 - 0.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 - 0.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 4950 HS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.15 - 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 - 0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.15 - 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 - 0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.15 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |
|||
Melt Flow | 0.15 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.15 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® E602 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding r.. |
|||
Melt Flow | 0.15 g/10 min | 0.15 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® E922 Film HDPE High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristi.. |