Physical Properties Metric English Comments
Melt Flow 0.055 g/10 min
0.055 g/10 min
Exxon Method (I2). HLMI (I21) is 9 g/10 min.
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
Melt Flow 0.055 g/10 min
0.055 g/10 min
Exxon Method (I2). HLMI (I21) is 9 g/10 min.
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...