Physical Properties Metric English Comments
Water Vapor Transmission 3000 g/m²/day

@Temperature 38.0 °C
193 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM D6701
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..