Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 3000 g/m²/day @Temperature 38.0 °C |
193 g/100 in²/day @Temperature 100 °F |
90% RH; ASTM D6701 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |