Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.900 g/m²/day @Temperature 23.0 °C |
0.0580 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 26MB768 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi.. |
|||
Water Vapor Transmission | 0.900 g/m²/day @Temperature 23.0 °C |
0.0580 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 26MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac.. |
|||
Water Vapor Transmission | 0.900 g/m²/day @Temperature 23.0 °C |
0.0580 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Water Vapor Transmission | 0.900 g/m²/day @Temperature 23.0 °C |
0.0580 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MH247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |
|||
Water Vapor Transmission | 0.900 g/m²/day @Temperature 25.0 °C |
0.0580 g/100 in²/day @Temperature 77.0 °F |
75% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 47MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |