Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.605 g/m²/day

@Temperature 23.0 °C
0.0390 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 40MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea..
Water Vapor Transmission 0.605 g/m²/day

@Temperature 23.0 °C
0.0390 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 40MB668 OPP Film
Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo..
Water Vapor Transmission 0.605 g/m²/day

@Temperature 23.0 °C
0.0390 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 50MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & ..