Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.605 g/m²/day @Temperature 23.0 °C |
0.0390 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 40MB666 OPP Film Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea.. |
|||
Water Vapor Transmission | 0.605 g/m²/day @Temperature 23.0 °C |
0.0390 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Bicor™ 40MB668 OPP Film Product Description: A high speed transparent biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides excellent perfo.. |
|||
Water Vapor Transmission | 0.605 g/m²/day @Temperature 23.0 °C |
0.0390 g/100 in²/day @Temperature 73.4 °F |
85% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 50MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & .. |