Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 69.5 SUS | 69.5 SUS | See Note 3. |
ChevronTexaco Polystar® CVJ Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Saybolt Viscosity at 210°F | 69.5 SUS | 69.5 SUS | |
ChevronTexaco Rykon® 1426 Premium Grease Chevron Rykon Premium Grease No. 1426 contains polyurea thickener, highly refined paraffinic base oil, rust and oxidation inhibiting additives, as well as heatstable extreme pressure additives.Appli.. |