Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 181 SUS | 181 SUS | |
ConocoPhillips Syncon® 460 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Saybolt Viscosity at 210°F | 181 SUS | 181 SUS | See Note 3. |
ChevronTexaco Marfak® 0 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |