ChevronTexaco Marfak® 0

Category Fluid , Lubricant , Organic Soap Gellant
Manufacturer ChevronTexaco Corp
Trade Name Marfak®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Marfak® 0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separation and protects against dirt and rust. Texaco Marfak grease is formulated to:Protect equipment from dust and dirt by providing a sealProtect equipment against rusting in the presence of small amounts of water.Texaco Marfak greases are recommended for slow speed, plain bearing and general-purpose lubrication of agricultural equipment.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 220927; MSDS Number: 9003
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 4853 SUS
4853 SUS
See Note 3.
Saybolt Viscosity at 210°F 181 SUS
181 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 880 cSt
880 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 37 cSt
37 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 370
370
Unknown Amount of Work, 25°C (77°F)
Oil Separation 1.7 %
1.7 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
See Note 2.
Minimum Service Temperature, Air -12.0 °C
10.4 °F
See Note 1.
Flash Point 220 °C
428 °F
See Note 3.
Dropping Point 166 °C
331 °F
Descriptive Properties Value Comments
Color Dark Brown
Rust Prevention Pass
Texture Stringy
Thickener, % 7
Sodium