Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 174 SUS | 174 SUS | |
ChevronTexaco Pinnacle® EP 320 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Saybolt Viscosity at 210°F | 174 SUS | 174 SUS | See Note 3. |
ChevronTexaco Starplex® HD 6802 NLGI Grade 2 Texaco Starplex HD 6802 delivers value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protecti.. |
|||
Saybolt Viscosity at 210°F | 174 SUS | 174 SUS | |
ChevronTexaco TEGRA® ISO 320 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |