ChevronTexaco Starplex® HD 6802 NLGI Grade 2

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Starplex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Starplex® HD 6802 NLGI Grade 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Starplex HD 6802 delivers value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protection.Protection against shock loading, thus extending bearing life.Outstanding film strength and adhesive properties.Texaco Starplex HD 6802 is a water resistant, extreme pressure grease.It is manufactured using highly refined, select high viscosity index base oils, and a lithium complex soap.Texaco Starplex HD 6802 is recommended for:General use in steel and paper mills.Off-road and industrial applications, such as construction and mining, where a higher base oil viscosity is preferred.Automotive applications, where low temperature performance is not critical.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 221936; MSDS Number: 9030
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 3845 SUS
3845 SUS
See Note 3.
Saybolt Viscosity at 210°F 174 SUS
174 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 705 cSt
705 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 36 cSt
36 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
Penetration P(60), 1/10 mm 280
280
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 163 °C
325 °F
See Note 2.
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
See Note 1.
Dropping Point 232 °C
450 °F
Descriptive Properties Value Comments
Color Brown
Texture Tacky
Thickener, % 10
Lithium Complex