Physical Properties Metric English Comments
API Gravity 28.5 °
28.5 °
ExxonMobil Mobil Aero HF
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
API Gravity 28.5 °
28.5 °
ChevronTexaco 220 Way Lubricant
Texaco Way Lubricants deliver value through:Excellent separation from metalworking coolants — The SKC (SKC Gleittechnik) coolant separation test showed excellent separation from a wide variety of c..
API Gravity 28.5 °
28.5 °
ChevronTexaco HDAX® SAE 40 Low Ash Gas Engine Oil
FeaturesChevron HDAX Low Ash Gas Engine Oils are high quality, bright stock-free, low ash, dispersant/detergent type engine oils.They are formulated with ISOSYN™ base stocks and an additive package..
API Gravity 28.5 °
28.5 °
ChevronTexaco ISO 220 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
API Gravity 28.5 °
28.5 °
ChevronTexaco Quenchtex® MM
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f..
API Gravity 28.5 °
28.5 °
ChevronTexaco Rando® HD 220
Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow..
API Gravity 28.5 °
28.5 °
ASTM D287
ChevronTexaco Regal® 220 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
API Gravity 28.5 °
28.5 °
ChevronTexaco Vistac® ISO 220 Way Oil D
FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with ..
API Gravity 28.5 °
28.5 °
ExxonMobil Mobil Aero HF
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
API Gravity 28.5 °
28.5 °
ASTM D287
ChevronTexaco Regal® 220
Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear ..