Physical Properties Metric English Comments
Pore Size 0.000400 - 0.000700 microns
0.0000157 - 0.0000276 mil
4 - 7 angstroms Diameter
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..