Physical Properties Metric English Comments
Apparent Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894
3M Dyneon™ TFM™ 1600 Modified PTFE Powder  (discontinued **)
Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio..
Apparent Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Apparent Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Apparent Bulk Density 0.830 g/cc
0.0300 lb/in³
ISO 60
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U..
Apparent Bulk Density 0.830 - 0.930 g/cc
0.0300 - 0.0336 lb/in³
Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ Plus 1111 PET Resin
Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un..
Apparent Bulk Density 0.830 - 0.930 g/cc
0.0300 - 0.0336 lb/in³
Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ Preserve 2201 PET Resin
Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento supe..
Apparent Bulk Density 0.830 - 0.930 g/cc
0.0300 - 0.0336 lb/in³
60 pellets/g, Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ Refresh 1101 PET Resin
Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen..
Apparent Bulk Density 0.830 - 0.950 g/cc
0.0300 - 0.0343 lb/in³
Average value: 0.890 g/cc Grade Count:5
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..