Physical Properties Metric English Comments
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
DIN 53 466
3M Dyneon™ TF 4212 PTFE 10% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
DIN 53 466
3M Dyneon™ TFM™ 4212 Modified PTFE, 10% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Apparent Bulk Density 0.770 - 1.02 g/cc
0.0278 - 0.0368 lb/in³
Average value: 0.878 g/cc Grade Count:5
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
ISO 60
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
ISO 60
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive  (discontinued **)
Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information..
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
ASTM D1895
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic
Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in ..
Apparent Bulk Density 0.770 g/cc
0.0278 lb/in³
ISO 60
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..