Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4212 PTFE 10% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | DIN 53 466 |
3M Dyneon™ TFM™ 4212 Modified PTFE, 10% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.770 - 1.02 g/cc | 0.0278 - 0.0368 lb/in³ | Average value: 0.878 g/cc Grade Count:5 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive
(discontinued **) Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information.. |
|||
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in .. |
|||
Apparent Bulk Density | 0.770 g/cc | 0.0278 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |