Physical Properties Metric English Comments
Apparent Bulk Density 0.530 - 0.590 g/cc
0.0191 - 0.0213 lb/in³
ISO 60:1977
BorsodChem ONGROVIL S-5064 Suspension PVC-Resin
S-5064 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r..