Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 50 is a low molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduce.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ FIT E 51 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 51 is a medium molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and red.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ FIT E 52 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 52 is a high molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduc.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 217 is a low to medium molecular weight homopolymer blending resin intended for use as a formulation tool in plastisol formulations.It improves air release performance resulting in reduced sc.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 (B) |
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An experimental, very high flow, 20% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/2 Polyolefin Catalyst CT/2 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it all.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/2-LR Polyolefin Catalyst CT/2-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it .. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/2-LR UV Polyolefin Catalyst CT/2-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds,.. |
|||
Apparent Bulk Density | 0.530 - 0.590 g/cc | 0.0191 - 0.0213 lb/in³ | ISO 60:1977 |
BorsodChem ONGROVIL S-5064 Suspension PVC-Resin S-5064 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
Arkema Group Lacovyl® GA 7701 H Vinyl Copolymer LACOVYL GA 7701 H is a copolymer of vinyl chloride and vinyl acetate produced by suspension polymerization process. It may be used by itself or blended with a PVC homopolymer of similar molecular we.. |
|||
Apparent Bulk Density | 0.530 g/cc | 0.0191 lb/in³ | |
Arkema Group Lacovyl® GA 7701 Vinyl Copolymer LACOVYL GA 7701 is a copolymer of vinyl chloride and vinyl acetate produced by suspension polymerization process. It may be used by itself or blended with a PVC homopolymer of similar molecular weig.. |
|||
Apparent Bulk Density | 0.529 g/cc | 0.0191 lb/in³ | ASTM D1895 (B) |
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |