Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.215 - 0.425 g/cc | 0.00777 - 0.0154 lb/in³ | Average value: 0.361 g/cc Grade Count:8 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |