Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.00900 - 0.650 g/cc | 0.000325 - 0.0235 lb/in³ | Average value: 0.0682 g/cc Grade Count:21 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | Average value: 0.576 g/cc Grade Count:17 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | MSZ ISO 60:1994 |
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS) ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e... |
|||
Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | MSZ ISO 60:1994 |
BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS) ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |
|||
Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | MSZ ISO 60:1994 |
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS) ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |
|||
Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | MSZ ISO 60:1994 |
BorsodChem ONGROSTYR F-III Expandable Polystyrene (EPS) ONGROSTYR F-III is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i... |