Polymer Property : Apparent Bulk Density = 0.00900 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.00900 g/cc
0.000325 lb/in³
On a continuous pre-expander after two expansions
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
Apparent Bulk Density 0.00900 g/cc
0.000325 lb/in³
On a continuous pre-expander after two expansions
Polimeri Europa Extir® LN 7000 Expandable Polystyrene
Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e..
Apparent Bulk Density 0.00900 - 0.650 g/cc
0.000325 - 0.0235 lb/in³
Average value: 0.0682 g/cc Grade Count:21
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..