Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® LN 5000 Expandable Polystyrene Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® LN 7000 Expandable Polystyrene Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **) Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Apparent Bulk Density | 0.0150 g/cc | 0.000542 lb/in³ | On a discontinuous pre-expander |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |