Physical Properties Metric English Comments
Apparent Bulk Density 0.0170 g/cc
0.000614 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® LN 2001 Expandable Polystyrene
Extir LN 2001 belongs to a new expandable product family, the Leonardo Series. Extir LN 2001 is specially coated to be incorporated into bricks, concrete, mortar and plaster, in order to lighten the..
Apparent Bulk Density 0.0170 g/cc
0.000614 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene  (discontinued **)
Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3..
Apparent Bulk Density 0.0170 g/cc
0.000614 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene  (discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
Apparent Bulk Density 0.0170 g/cc
0.000614 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene  (discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Apparent Bulk Density 0.0170 g/cc
0.000614 lb/in³
On a discontinuous pre-expander
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene  (discontinued **)
Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200..