Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | <= 4000 µm | <= 4000 µm | |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |