Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | <= 149 µm | <= 149 µm | |
Chosun Refractories FAM-1 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Grain Size | <= 149 µm | <= 149 µm | |
Chosun Refractories FAM-2 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |