Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 950 - 975 cP | 950 - 975 cP | ASTM D2293 |
Fibre Glast 2000 / 2020 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Viscosity | 950 cP @Temperature 25.0 °C |
950 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8118 Silicone Stabilizer for PU Foam STRUKSILON 8118 is a silicone stabilizer for liquid-CO2 of medium potency for the production of flexible polyurethane slabstock foam based on polyether polyols.Applications: STRUKSILON 8118 was espe.. |
|||
Viscosity | 950 cP @Temperature 25.0 °C |
950 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8002 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8002 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU 1- or 2-component spray foam applications.Applications: Inf.. |
|||
Viscosity | 950 cP @Temperature 25.0 °C |
950 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8027 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8027 is a specifically designed silicone stabilizer for appliance application and other applications where good flowability is required, like pipe insulation and hot water boiler producti.. |
|||
Viscosity | 950 cP @Temperature 25.0 °C |
950 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8030 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8030 is a universal stabilizer for the production of polyurethane rigid foams. Due to its excellent flow properties and the very good insulation values that can be achieved STRUKSILON 803.. |