Struktol STRUKSILON 8027 Silicone Stabilizer for PU-Rigid Foam

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name STRUKSILON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol STRUKSILON 8027 Silicone Stabilizer for PU-Rigid Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
STRUKSILON 8027 is a specifically designed silicone stabilizer for appliance application and other applications where good flowability is required, like pipe insulation and hot water boiler production.Applications: Information provided by Struktol
Physical Properties Metric English Comments
Density 1.045 g/cc
0.03775 lb/in³
approximation
Viscosity 950 cP

@Temperature 25.0 °C
950 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Optical Properties Metric English Comments
Refractive Index 1.4465

@Temperature 25.0 °C
1.4465

@Temperature 77.0 °F
Descriptive Properties Value Comments
Appearance Clear, colorless to slightly yellow liquid